Titanium Grade 7
Titanium Grade 7 is the most resistant to corrosion in reducing acids with physical/mechanical properties equivalent to Gr. 2. Grade 7 also has excellent weldability and fabricability.
Available forms are seamless pipe, welded pipe, seamless tube, welded tube, bar, wire, sheet, plate, forgings, pipe fittings and flanges.
Titanium Grade 7 Specification
|
Sheet/Plate content |
ASME SB-265 |
Round Bar/Wire content |
ASME SB-348 |
Pipe content |
ASME SB-337, ASME SB-338 |
Tube content |
ASME SB-337, ASME SB-338 |
Fittings content |
ASME SB-363 |
Forgings content |
ASME SB-381 |
Titanium Grade 7 Chemical analysis
|
C (Carbon content) |
.08 max |
N (Nitrogen content) |
.03 max |
O (Oxygen content) |
.25 max |
H (Hydrogen content) |
.015 max |
| Pd |
.12 - .25 |
Cr | |
Ni | |
Mo | |
Cu | |
Co | |
V (Vanadium content) |
|
Ti (Titanium contenet) |
bal |
Al (Aluminum content) |
|
Fe (Iron content) |
0.30 max |
Nb (Niobium content) |
|